Material Notes:
Chain making. Palladium has been used to create casting alloys at various levels of fineness. Palladium produces a softer casting.
Physical Properties Metric English Comments
Density 19.1 g/cc
0.690 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 64
64
As Cast
90
90
Annealed
Elongation at Break 22 %
22 %
Annealed
22 %
22 %
As Cast
Thermal Properties Metric English Comments
Melting Point 1730 - 1750 °C
3150 - 3180 °F
Solidus 1730 °C
3150 °F
Liquidus 1750 °C
3180 °F
Component Elements Properties Metric English Comments
Palladium, Pd 15 %
15 %
Platinum, Pt 85 %
85 %