Material Notes:
Features:Specifically designed for mass transit industriesCompliant with SMP800CMeets flamespread and smoke density requirements for mass transitExcellent formability and fabrication qualityGood definitionAllows for tight tolerancesEasy trimmingSuggested Applications:Seat backsBulkhead componentsWindow revealCeiling componentsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength 23.4 MPa
3390 psi
ASTM D638
Tensile Modulus 2.261 GPa
327.9 ksi
ASTM D638
Flexural Strength 42.6 MPa
6180 psi
ASTM D790
Flexural Modulus 2.71 GPa
393 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
annealed; ASTM D648
Descriptive Properties Value Comments
Flammability, Radiant Panel Pass
ASTM E162
Smoke Generation Pass
ASTM E662
Toxicity Requirements Pass
SMP 800C