Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible D9002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Therma-Tech™ NJC-6000 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Specific Gravity | 1.58 - 1.64 g/cc | 1.58 - 1.64 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 08/26-FC-LMP Beige Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Sylvin Technologies 9999-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 313AR Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Tufflake® 5950 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 454 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3000 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3000 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Mixed |
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Mixed |
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Mixed |
Tra-Con Tra-Cast F353 Optically Opaque Casting System TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D 792 |
RTP Company RTP 1400 AG-330 Polyethersulfone (PES), Glass Fiber |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D 792 |
RTP Company ESD 805 Acetal (POM), Glass Fiber - ESD Protection - Electrically Conductive |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Celanese Celcon® GC25TF POM, 25% Glass Reinforced Celcon« GC25TF is a 25% glass coupled acetal copolymer formulated for higher flow in thin walled and small parts. Celcon GC25TF is also exceptionally resistant to fuel. It offers excellent resista.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Cheng Yu Plastic E2320 Flame Retardant PET, 20% Glass Fiber |
|||
Specific Gravity | 1.58 - 1.62 g/cc | 1.58 - 1.62 g/cc | ASTM D-792 |
Axiall PURGOVIN® 3000 Rigid PVC, Extrusion Georgia Gulf PURGOVIN® 3000 is a unique vinyl based powder blend purging compound designed for use in the shutdown or cleaning of extrusion lines. Purgovin® offers excellent heat stability and ca.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Dry; ASTM D792 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Celanese Celcon® GC25A POM, 25% Glass Reinforced Celcon« acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
RTP Company RTP 4008A Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 45%
(discontinued Glass Fiber 45%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Mixed; TM R050-16 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |