Karina 10/70-IE White Color Concentrate MBU

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 10/70-IE White Color Concentrate MBU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVA based color concentrate, with 70% of titanium dioxide, recommended for application in polyolefinic and PVC compounds for general purposes. Minimum recommended usage of 0.5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.95 - 2.01 g/cc
1.95 - 2.01 g/cc
ASTM D 792
Moisture Absorption <= 0.100 %
<= 0.100 %
ME-52
ASTM Color -1.51 - 0.090
-1.51 - 0.090
Color A, ME 12
-0.900 - 0.70
-0.900 - 0.70
Color B, ME 12
93.18 - 94.78
93.18 - 94.78
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 43 - 47

@Time 15.0 sec
43 - 47

@Time 0.00417 hour
ASTM D 2240
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application Blow Molding
Extrusion
Injection