Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 1.00e+14 ohm-cm | <= 1.00e+14 ohm-cm | Teil 30; IEC 600093 / VDE 0303 |
Okulen® 2000 PE-UHMW, AB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Volume Resistivity | <= 1.00e+14 ohm-cm | <= 1.00e+14 ohm-cm | Teil 30; IEC 600093 / VDE 0303 |
Okulen® 2000 PE-UHMW, DG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | DIN 53482 |
Qualchem Danamid FES Polyamide 6 Impact resistant, dryInformation provided by Qualchem Zrt. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D 257 |
RTP Company RTP 4007 TFE 10 Polyphthalamide (PPA), Glass Fiber - PTFE Lubricated |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D 257 |
Karina Karintox ENCH./03 Polyolefin Compound Karintox is a thermoplastic polyolefin, flame retardant, non-halogen, and low smoke emission. Recommended for electrical coating for cables until 1KV. For a better usage/processing, a pre-warm/heat .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Kolon KOCETAL® K100 Standard Grade Acetal Resin Suitable for extrusion and injection molding of thick products. Applications: Extruded use such as rod, pipe, tube, and sheetInformation provided by API Kolon. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Lanxess Durethan® B 40 FKA 000000 Nylon 6, Film Grade PA 6 film grade of high viscosity, nucleated and lubricated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE composite films |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | NBR 5403 |
Karina E 18/89-FC-LMP Gray Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PA6 FR-N Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and heat StabilizedProcessin.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 04003 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PC MRX BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® POM CO X Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Saint-Gobain COHRlastic® TC100U Uncured Thermally Conductive Solid Silicone Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | |
Master Bond EP21NDFG Two component epoxy compound for high performance applications Product Description: Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | ASTM D 257 |
RTP Company RTP 227 A Nylon 6 (PA), Mineral |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 23.0 °C |
1.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 87/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® M25-45 Acetal Co-polymer (POM), Weather resistance, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | CEI 60093 |
Addiplast Addilene J 326 V30 Polypropylene Copolymer High modulus, high durabilityInformation provided by Addiplast. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
PolyOne Edgetek® AT-10GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc. |