Karina 550D32/13-AT-IS Orange PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 550D32/13-AT-IS Orange PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.14 - 1.20 g/cc
1.14 - 1.20 g/cc
ASTM D 792
ASTM Color 41.17 - 47.17
41.17 - 47.17
Color B, ME 12
41.4 - 47.4
41.4 - 47.4
Color A, ME 12
49.61 - 55.61
49.61 - 55.61
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Descriptive Properties Value Comments
Application Packaging/Stopper Seals