Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E TR 500D22/173 Honey PVC Compound Honey PVC compound additivated with nitrile rubber, recommended for injection of general soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | NBR NM-IEC 60811-1-1 |
Karina E TR-652D48/1-B-IS Black PVC Compound PVC Compound with NBR; recommended for injection of automotive parts and extrusion of flexible jacket for electrical cables.Information provided by Karina Indústria e Comércio de Plásticos .. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina FADA 45-YAT White PVC Compound Non-toxic PVC compound recommended for injection of inseminator for veterinary applicationsInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D32/13-AT-IS Orange PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D35/1-AT-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D42/10-AT-IS Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 550D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 603-48/1-Y-BZ Black PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 650D08/244-D-IS Beige PVC Compound Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 650D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 651-48/1-B-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for extrusion and injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 752-12/6-Y-BZ Ruby Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 52/205-D-AT-IS Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 650D48/1 Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 670D10/116-Y White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 670D35/1-A-AT-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 680D48/1-G-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina E 801D06/418-C Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 7.85 MPa | >= 1140 psi | ASTM D 638 |
Karina 600D48/1-C-IS Black PVC Compound PVC Compound recommended for injection of automotive parts and extrusion of flexible jacket for electrical cablesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 7.85 MPa | 1140 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well .. |