Material Notes:
PVC compound recommended for extrusion of notebook spiresInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.37 g/cc
1.31 - 1.37 g/cc
ASTM D 792
ASTM Color -1.56 - 1.44
-1.56 - 1.44
Color B, ME 12
-1.54 - 1.46
-1.54 - 1.46
Color A, ME 12
0.00 - 2.0
0.00 - 2.0
Delta E, ME 12
25.59 - 28.59
25.59 - 28.59
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles