Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ISO 1183 |
S&E Specialty Polymers TufTech™ SE11-031 PVC Compound Application: Automotive - PVC, Integral Colored, Exterior Weatherable, Extrusion & Injection Molding CompoundInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 898-08/175-IS-RG Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 898-10/137-IS-RG White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 898-10/161-IS-RG White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 800-21/9-IS-RG Coke PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 800-48/1-IS-RG Black PVC Compound PVC compound recommended for extrusion of notebook spiresInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 801-27/13-IS-RG Smoky Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 830-21/9-IS-RG Coke PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 846-10/114-IS-RG White PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 846-32/64-IS-RG Orange PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 858-12/20-IS-RG PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 861-40/27-IS-RG Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 105852-35/1-A-IS-L Ivory PVC Compound PVC compound recommended for extrusion of wires THHN and THWN.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.37 g/cc | 1.30 - 1.37 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 75800-35/1-B-AC Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 805-48/1-IS-RG Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 836-10/132-IS-RG White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 15644 Wire & Cable Flexible PVC Semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 16881 Coax & Telecom Flexible PVC 90C rated, non-lead stabilized jacket compound with excellent low temperature properties. Suitable for riser and optical fiber constructions.Information provided by Georgia GulfGeorgia Gulf became .. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19930 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 22851 Coax & Telecom Flexible PVC Non-lead stabilized, flame retardant jacket compound. Best suited for CM, CMR applications over FR PVC. Maximum service temperature rating of 75°C. UL recognized for 720 hr sunlight resistance.I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8916 Moldings & Extrusions Flexible PVC A satin finish extrusion compound best suited for extruded T-moldings, tubings and other shapes where uniform flow through the die is required. The compound exhibits excellent abrasion resistance.I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8922 Moldings & Extrusions Flexible PVC A general purpose, matte finish, extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19850 Moldings & Extrusions Flexible PVC Primary insulation compound recommended for 105C, 1/32 wall and larger applications. Also well suited for plug molding. UL rated 94 HB.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 390 Coax & Telecom Flexible PVC Buried service telecom jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 48562 Moldings & Extrusions Flexible PVC Automotive window encapsulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 50898 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 802-27/13-IS-RG Smoky Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 4520 Flexible PVC Non-lead stabilized, thin wall, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8911 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound. UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |