Karina 804-02/69-Y-RTC Yellow PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 804-02/69-Y-RTC Yellow PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.43 g/cc
1.37 - 1.43 g/cc
ASTM D 792
ASTM Color -5.35 - -2.35
-5.35 - -2.35
Color A, ME 12
78.63 - 81.63
78.63 - 81.63
Color B, ME 12
83.43 - 86.43
83.43 - 86.43
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Thermal Properties Metric English Comments
Brittleness Temperature <= -41.0 °C
<= -41.8 °F
ASTM D 638
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Application Electrical Conduit