Material Notes:
Weather resistant and flame retardant PVC compound, class 70CInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.43 - 1.49 g/cc
1.43 - 1.49 g/cc
NBR NM-IEC 60811-1-3
ASTM Color 22.67 - 25.67
22.67 - 25.67
Color A, ME 12
40.13 - 43.13
40.13 - 43.13
Color B, ME 12
73.97 - 76.97
73.97 - 76.97
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92

@Time 15.0 sec
88 - 92

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 17.7 MPa
>= 2560 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 150 %
>= 150 %
NBR NM-IEC 60811-1-1
Thermal Properties Metric English Comments
Oxygen Index >= 30 %
>= 30 %
NBR 6245
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application -40 Grades/+105 Grades
70 Grades