Material Notes:
Heavy metal free PVC compound recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.42 - 1.48 g/cc
1.42 - 1.48 g/cc
ASTM D 792
ASTM Color -1.61 - -0.0100
-1.61 - -0.0100
Color A, ME 12
-1.39 - 0.21
-1.39 - 0.21
Color B, ME 12
91.43 - 93.03
91.43 - 93.03
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 55.9 MPa
>= 8110 psi
ASTM D 638
Modulus of Elasticity >= 3.29 GPa
>= 477 ksi
ASTM D 638
Izod Impact, Notched >= 0.380 J/cm
>= 0.712 ft-lb/in
Method A; ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 80.0 °C
>= 176 °F
ASTM D 1525
Heat Distortion Temperature >= 76.0 °C
>= 169 °F
ASTM D 648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Application General Purpose Profiles