Kazanorgsintez 158BK-15 Low Density Polyethylene Composite

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 158BK-15 Low Density Polyethylene Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Produced from low density polyethylene grades 15803-020 and 15813-020. Application: Designed for production of sealing coatings on industrial items.Information Provided by Kazanorgsintez
Mechanical Properties Metric English Comments
Elongation at Break >= 300 %
>= 300 %
Tear Strength Test >= 6.5
>= 6.5
MPa
Thermal Properties Metric English Comments
Softening Point 105 - 120 °C
221 - 248 °F
Minimum Service Temperature, Air <= -60.0 °C
<= -76.0 °F
Descriptive Properties Value Comments
Amount of impurities [pcs] 50