Kazanorgsintez E-18 Petroleum Resin

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez E-18 Petroleum Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic hydrocarbons.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density >= 0.800 g/cc

@Temperature 20.0 °C
>= 0.0289 lb/in³

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 25.0 °C
>= 77.0 °F
Initial
<= 320 °C
<= 608 °F
End
Component Elements Properties Metric English Comments
Free Water <= 3.0 %
<= 3.0 %
Descriptive Properties Value Comments
Appearance Liquid of yellow to dark-brown color