Kennametal Stellite Delcrome 253 Iron Alloy

Category Metal , Ferrous Metal , Superalloy
Manufacturer Kennametal Stellite
Trade Name Delcrome
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Delcrome 253 Iron Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Corrosion resistant alloys with moderate to high metal to metal wear resistance.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 36
36
Component Elements Properties Metric English Comments
Carbon, C <= 16.5 %
<= 16.5 %
Chromium, Cr 28 %
28 %
Iron, Fe >= 47.45 %
>= 47.45 %
as balance
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 4.5 %
4.5 %
Silicon, Si 1.3 %
1.3 %
Tungsten, W <= 1.75 %
<= 1.75 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition