Kennametal Stellite Deloro® 55 Nickel Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Deloro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Deloro® 55 Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This gas-atomized powder is highly spherical particles with very low gas content. The alloy exhibits hard chromium borides and carbides in a nickel rich matrix. The alloy has excellent resistance to abrasion and good deposition characteristics.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 52 - 57
52 - 57
Component Elements Properties Metric English Comments
Boron, B 2.7 %
2.7 %
Carbon, C 0.60 %
0.60 %
Chromium, Cr 12 %
12 %
Iron, Fe 4.0 %
4.0 %
Nickel, Ni >= 76.7 %
>= 76.7 %
as balance
Silicon, Si 4.0 %
4.0 %
Descriptive Properties Value Comments
Application Technique HVOF & thermal spray
PTA & laser deposition
Spray-fuse & powder welding