Kennametal Stellite Nistelle C276 Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Nistelle
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Nistelle C276 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This alloy has excellent resistance to a wide variety of chemical process environments, including strong oxidizers such as ferric and cupric chlorides, hot contaminated media (organic and inorganic), chlorine, formic and acetic acids, acetic anhydride, and seawater and brine solutions. It is used in flue gas desulfurization systems because of its excellent resistance to sulfur compounds and chloride ions encountered in most scrubbers. Nistelle C-276 alloy has excellent resistance to pitting and to stress-corrosion cracking. It is also one of the few materials that can withstand the corrosive effects of wet chlorine gas, hypochlorite and chlorine dioxide.Information provided by Kennametal Stelliteâ„¢
Component Elements Properties Metric English Comments
Chromium, Cr 15.5 %
15.5 %
Iron, Fe 5.5 %
5.5 %
Molybdenum, Mo 16 %
16 %
Nickel, Ni >= 58.15 %
>= 58.15 %
as balance
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 3.7 %
3.7 %
Vanadium, V 0.15 %
0.15 %
Descriptive Properties Value Comments
Application Technique HVOF & thermal spray
PTA & laser deposition