Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Kolon
Trade Name ELLAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength 43.1 MPa
6260 psi
ASTM D412
Tensile Stress 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Tear Strength 108 kN/m
616 pli
ASTM D624
Processing Properties Metric English Comments
Nozzle Temperature 170 - 180 °C
338 - 356 °F
Injection Molding
Zone 1 150 - 170 °C
302 - 338 °F
Injection Molding
155 - 165 °C
311 - 329 °F
Extrusion Molding
Zone 2 160 - 170 °C
320 - 338 °F
Extrusion Molding
170 - 180 °C
338 - 356 °F
Injection Molding
Zone 3 165 - 175 °C
329 - 347 °F
Extrusion Molding
170 - 180 °C
338 - 356 °F
Injection Molding
Zone 4 165 - 175 °C
329 - 347 °F
Extrusion Molding
Die Temperature 165 - 175 °C
329 - 347 °F
Extrusion Molding
Head Temperature 170 - 180 °C
338 - 356 °F
Extrusion Molding