Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 165 - 175 °C | 329 - 347 °F | Extrusion Molding |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |
|||
Zone 3 | 165 - 170 °C | 329 - 338 °F | |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
Zone 3 | 165 - 175 °C | 329 - 347 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten.. |
|||
Zone 3 | 165 °C | 329 °F | |
Lubrizol Estane® ALR G500 Water Absorbent Thermoplastic Polyurethane Type: Estane® ALR G500 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provide.. |