Material Notes:
KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very similar to rubber, but its processability is much superior to rubber. While its flexibility and elastic recovery are similar to rubber, its mechanical properties-heat resistance, weather resistance and UV stability-are far greater than the performance of rubber.Excellent flexibility and creep resistance, good mechanical properties and heat stability, good chemical resistanceInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.70 %
0.70 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Melt Flow 12 g/10 min

@Temperature 190 °C
12 g/10 min

@Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
DIN 53505; ASTM D2240
Tensile Strength, Ultimate 24.5 MPa
3560 psi
DIN 53455; ASTM D638
Elongation at Break 850 %
850 %
DIN 53455; ASTM D638
Flexural Yield Strength 49.0 MPa
7110 psi
DIN 53455; ASTM D790
Resilience 67
67
Izod Impact, Notched NB
NB
DIN 53453; ASTM D256
NB
NB
Low Temp
Taber Abrasion, mg/1000 Cycles 3.0
3.0
CS-17 WHEEL; ASTM D1044
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C
149 °F
DIN 53461; ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
Solenoid Brittle Point; ASTM D746
Flammability, UL94 HB
HB
measured in KOLON R&D Center