Polymer Property : Tensile Strength, Ultimate = 24.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.5 MPa
3560 psi
DIN 53455
Polikim ULPOLEN® 1000 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
DIN 53455
Polikim ULPOLEN® 300 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
DIN 53455
Polikim ULPOLEN® 500 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
DIN 53455; ASTM D638
Kolon KOPEL® KP3340 General Purpose TPE Resin
KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D638
KKPC Kuhmo HF400 Flame Retarded General Purpose HIPS
Key features: Translucent Injection. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resista..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D638
KKPC Kuhmo HF401 Flame Retarded General Purpose HIPS
Key features: High-fluidity. Common Uses: Office appliances.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and h..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D638
KKPC Kuhmo HFH 403 Flame Retarded HIPS
Key features: Low flammable V-2 grade. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D638
KKPC Kuhmo HFH 405 Flame Retarded HIPS
Key features: Non-halogen type. Common Uses: Parts needing non-halogen type.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
Shinil Chemical SHINNANO PP Polymer Nanocomposite IP
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
Shinil Chemical SHINSTRA PP SE3501 Structural Polymer Bumper
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D412
SK Chemicals SKYTHANE® 865A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D412
SK Chemicals SKYTHANE® T865A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D412
SK Chemicals SKYTHANE® UB410 Powder Coating
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D412
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D412
Lubrizol Estane® T370A Thermoplastic Polyurethane
Type: Estane® T370A is a Shore 74A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Tensile Strength, Ultimate 24.5 MPa
3550 psi
ISO 527
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper..
Tensile Strength, Ultimate 24.5 MPa
3550 psi
508 mm/min; ASTM D638
Dow Engage® 8440 Polyolefin Elastomer
Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer ..
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D638
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang.