Kostat 1940 Conductive PC Compound

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Kostat
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kostat 1940 Conductive PC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOSTAT 1940 is a conductive thermoplastic compound based on Polycarbonate and a special carbon fiber. KOSTAT 1940 is not dependant on atmospheric conditions and is used for ESD injection molded products.Special FeaturesThis product exhibits high conductivity, easy processing, smooth sheet surface, and tight dimensional tolerances after injection molding. This makes KOSTAT 1940 suitable for various injection molding applications.Applications:KOSTAT 1940 is recommended for electronics packaging such as ESD Trays and other injection molded products.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 160 MPa
23200 psi
ASTM D790
Flexural Modulus 7.95 GPa
1150 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
Kostat Rv
Surface Resistivity per Square 10000 ohm
10000 ohm
Kostat Rs
Processing Properties Metric English Comments
Rear Barrel Temperature 280 °C
536 °F
Middle Barrel Temperature 290 °C
554 °F
Front Barrel Temperature 300 °C
572 °F
Nozzle Temperature 290 °C
554 °F
Mold Temperature 80.0 °C
176 °F