Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1161 E (SIS) Linear Triblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1161 E (SIS) Linear Triblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1161 E is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from Europe in the physical form identified: D1161 ES - supplied as porous pellets dusted with silicaD1161 EU - supplied as undusted porous pelletsD1161 ESM - supplied as powder dusted with amorphous silicaRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1161 E is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 2781
Bulk Density 0.350 g/cc
0.0126 lb/in³
ASTM D1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Molecular Weight 207000 - 237000 g/mol
207000 - 237000 g/mol
KM 01
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 0.20 %
<= 0.20 %
EU; ISO 247
0.10 - 0.40 %
0.10 - 0.40 %
ESM; ISO 247
0.10 - 0.40 %
0.10 - 0.40 %
ET; ISO 247
2.5 - 5.0 %
2.5 - 5.0 %
ESM; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 30

@Time 30.0 sec
30

@Time 0.00833 hour
Measured on compression molded slabs; ISO 868
Tensile Strength 28.0 MPa
4060 psi
Measured on films cast from a toluene solution; ISO 37
Elongation at Break 1300 %
1300 %
Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.000900 GPa
0.131 ksi
Measured on films cast from a solution in toluene; ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.06%, primary phenolic antioxidant, KM 08
Polystyrene
13.5-16.5%, KM 03
Total Extractables
<1.0%, KM 05
Coupling Efficiency 78-84%
KM 01
Users viewing this material also viewed the following: