Physical Properties Metric English Comments
Molecular Weight 207000 - 237000 g/mol
207000 - 237000 g/mol
KM 01
Kraton® D1161 E (SIS) Linear Triblock Copolymer
Description: Kraton D1161 E is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from Europe in the physical form identified: D1161 E..