Kraton® D1161 J (SIS) Linear Triblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1161 J (SIS) Linear Triblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in the grade nomenclature: D1161 JSP - supplied as dusted dense pelletsD1161 JS - supplied as dusted crumbD1161 JU - supplied as undusted crumbRegion: Japan Uses: Kraton D1161 J Polymer is used in formulating adhesives, sealants and coatings. It is also used as a modifier of bitumen and polymers and in formulating compounds.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Volatiles <= 1.0 %

@Temperature 110 °C,
Time 7200 sec
<= 1.0 %

@Temperature 230 °F,
Time 2.00 hour
Viscosity 900 - 1700 cP
900 - 1700 cP
25% Toluene Solution at 25°C; KM 06
Melt Flow 1.3 - 3.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 - 3.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Ash <= 1.0 %
<= 1.0 %
JU; ISO 247
<= 1.0 %
<= 1.0 %
JSP; ISO 247
<= 2.5 %
<= 2.5 %
JS; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 37

@Time 30.0 sec
37

@Time 0.00833 hour
ISO 7619
Tensile Strength 28.0 MPa
4060 psi
ISO 37
Elongation at Break 1300 %
1300 %
ISO 37
300% Modulus 0.000900 GPa
0.131 ksi
ISO 37
Descriptive Properties Value Comments
Content Bound Styrene
15 percent
Users viewing this material also viewed the following: