Melt Flow 2.4 - 3.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.4 - 3.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1500J (T30G) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 1.3 - 3.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 - 3.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Kraton® D1161 J (SIS) Linear Triblock Copolymer
Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t..