Material Notes:
Description: Kraton D1163 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified: Kraton D1163 PT - supplied as a dusted dense pelletKraton D1163 PTM - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton D1163 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationNote 1) The final dusting level is a combination of the talc from the original D1163PT plus silica added during the milling process.Information provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Viscosity 900 cP
900 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow 23 g/10 min

@Load 5.00 kg,
Temperature 200 °C
23 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.25 - 0.45 %
0.25 - 0.45 %
PT, Talc; BAM 908
2.5 - 5.0 %
2.5 - 5.0 %
PTM, See note 1); ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 25

@Time 10.0 sec
25

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 10.34 MPa
1500 psi
Typical properties of film cast from toluene solution; ASTM D412
Elongation at Break 1400 %
1400 %
Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.000430 GPa
0.0624 ksi
Typical properties of film cast from toluene solution; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 38 %
38 %
Descriptive Properties Value Comments
Content Antioxidant
0.08-0.3%, KM 08
Polystyrene
13.3-16.3%, KM 03
Total Extractables
<1.0%, KM 05
Styrene/Rubber Ratio 15/85