Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000430 GPa | 0.0624 ksi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® D1163 P (SIS) Linear Triblock Copolymer Description: Kraton D1163 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |