Material Notes:
Description: Kraton D1192 A is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms described: Kraton D1192 AT - supplied as porous pellets dusted with talcKraton D1192 AS - supplied as porous pellets dusted with amorphous silicaKraton D1192 ASM - supplied as powder dusted with amorphous silicaKraton D1192 ATM - supplied as powder dusted with talc for the North American marketRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D1192 A is used for modification of industrial and paving bitumen. It may also be suitable for use in formulating adhesives, sealants and coatings, and in the modification of polymers.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Molecular Weight 138000 - 162000 g/mol
138000 - 162000 g/mol
Triblock
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.10 - 0.40 %
0.10 - 0.40 %
AS, AT; ISO 247
2.5 - 5.0 %
2.5 - 5.0 %
ASM; ISO 247
4.0 - 6.0 %
4.0 - 6.0 %
ATM; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 15.0 sec
70

@Time 0.00417 hour
Measured on compression molded slabs; ASTM D2240
Descriptive Properties Value Comments
Content Antioxidant
>0.16%, KM 08
Polystyrene
28.5-32.5%, KM 03
Total Extractables
<1.0%, KM 05
Vinyl
>35%, KM 03
Triblock Content >90%
KM 01