Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Loose |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Nabaltec APYRAL® AOH 60 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature applicationsLow sedimentation at good viscosity performance in resinsGood ch.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
PolyOne Geon™ 180 Series 180X5 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 180X5 is low molecular weight resin that provides good chemical foam characteristics with excellent overblow resistence. The modified rheology of Geon® 180X5 provides increased viscosity and.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
PolyOne Geon™ 180 Series 186A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 186A is low molecular weight homopolymer resin, providing a good balance of fused film physical properties and fusion characteristics. It provides excellent chemical foam characteristics with.. |
|||
Bulk Density | <= 0.400 g/cc | <= 0.0145 lb/in³ | |
Magyar Aluminum ALOLT 59AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Magyar Aluminum ALO-P90-06 Alumina Alumina for Polishing |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1152 E (SBS) Liner Block Copolymer Description: Kraton D1152 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1153 E (SBS) Liner Block Copolymer Description: Kraton D1153 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1191 E (SBS) Radial Block Copolymer Description: Kraton D1191 E is a clear, radial block copolymer based on styrene and butadiene with bound styrene of 33.5% mass. It is supplied from Europe in the physical forms described: Kraton D11.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1192 A (SBS) Liner Block Copolymer Description: Kraton D1192 A is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms described: Kraton D1192 .. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D4153 E (O/E SBS) Linear Block Copolymer Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is cl.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Tap Density |
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder Crystalline hexagonal platelet morphology. AC6041 shows good dispersion, with enhanced lubricity and thermal properties. AC6041 powder is readily used in the production of many advanced materials... |
|||
Bulk Density | 0.400 g/cc @Temperature 200 °C |
0.0145 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ SLG Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Solvay GEROPON® T/36 Surfactant Identification: SODIUM POLYCARBOXYLATESolubility: Soluble in water. Insoluble in polar and aromatics solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Dispers.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Trelleborg Fillite® 160W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF Hydroxypivalic Acid Neopentylglycolester (HPN Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester (HPN) is a colorless, odorless solid.Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopentyl hydroxypiva.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
BCC Products BC 37 Ceramic Microspheres BC 37 are hollow microspheres, which are ceramic in nature. They are an efficient lightweight filler material to be used in applications with most resins.Information provided by BCC Products, Inc. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D4895 |
3M Dyneon™ J24 PTFE 3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and applic.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF 2-Methyl Imidazole Pure Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazolApplications: Intermediate used in Pharmac.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
BASF Heligoen® Blue K 6850 Color Additive Chemical Structure: Cu-Phthalocyanine alpha instab.Application: Colourant for plastics; PVC-p, PVC-u and UPRecommendations for food applications: BgVV, FDA, FrancePhysical form: PowderInformation pr.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D4895 |
3M Dyneon™ TF 9205 PTFE 3M™ Dyneon™ PTFE TF micropowders can be used as additives in many different applications and at concentrations typically from 5 to 20%. Homogeneous incorporation helps ensure optimum performance. .. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Loose |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Solvay SUPRAGIL® WP Sodium Isopropyl Naphthalene Sulfonate Sodium Isopropyl Naphthalene Sulfonate. Multipurpose, low foaming wetting agent.Identification: DIALKYL NAPHTHALENE SULPHONATE SODIUM SALTCAS: 1322 – 93 -6Solubility: Soluble in water. Insoluble in.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 1132P Cellulose Reinforced Phenolic Novolac FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Militar.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D4745 |
3M Dyneon™ CC132 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a 10% carbon filled PTFE.Information provided by Dyneon, A 3M Company |