Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kureha KF Polymer 1700 High Viscosity PVDF Homopolymer

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Kureha
Trade Name KF Polymer
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kureha KF Polymer 1700 High Viscosity PVDF Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF polymer is being used in applications where heat resistance, anticorrosion, and weather-resistance are important.Typical Applications:Chemical valves, Pump part, & FittingsBinder for lithium ion batteriesHollow fiber for filtration of city water and sewageFilm & SheetInformation provided by Kureha.
Physical Properties Metric English Comments
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Viscosity 9100 cP

@Shear Rate 50.0 1/s,
Temperature 260 °C
9100 cP

@Shear Rate 50.0 1/s,
Temperature 500 °F
Melt; ASTM D3835
Viscosity Test 170 cm³/g

@Temperature 30.0 °C
170 cm³/g

@Temperature 86.0 °F
Inherent Viscosity in DMF Solution
Melt Flow 1.7 g/10 min

@Load 21.6 kg,
Temperature 230 °C
1.7 g/10 min

@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 173 °C
343 °F
ASTM D3418
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1e+14 - 1e+15 ohm-cm
1e+14 - 1e+15 ohm-cm
ASTM D257
Users viewing this material also viewed the following: