Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1e+14 - 1e+15 ohm-cm | 1e+14 - 1e+15 ohm-cm | ASTM D257 |
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Volume Resistivity | 1e+14 - 1e+15 ohm-cm | 1e+14 - 1e+15 ohm-cm | ASTM D257 |
Kureha KF Polymer 1700 High Viscosity PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |