Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LP170G PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LP170G PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from LP170G have low level of pinhole formation and have excellent whiteness and mechanical propertyMain Applications: Glove, DippingCAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.406 g/cc
1.406 g/cc
Bulk Density 0.290 - 0.390 g/cc
0.0105 - 0.0141 lb/in³
ASTM D1895
Volatiles <= 1.5 %

@Temperature 110 °C,
Time 3600 sec
<= 1.5 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 3000 - 4000 cP
3000 - 4000 cP
DOP 60phr, 6RPM; ASTM D1824-90
Viscosity Measurement >= 1.0

@Pressure 0.400 MPa
>= 1.0

@Pressure 58.0 psi
[g/sec], DOP 60phr, Severs; ASTM D1823-90
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 1600-1700
30°C, JIS K6721-77
K-Value 76
DIN53726
Copyright © lookpolymers.com All Rights Reserved