Zircar Refractory Composites RS-MS ALUMINA MOLDABLE SLEEVING

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Zircar Refractory Composites, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Refractory Composites RS-MS ALUMINA MOLDABLE SLEEVING.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ZIRCAR Refractory Sheet Type RS-MS Moldable Sleeving is a moist woven alumina composite sleeving. It is supplied in a wet form ready for the fabrication of custom shapes. It can be cut to size with a knife or scissors, wrapped around a suitable form, air dried, and immediately put into service. It is ideal for applications up to up to 1300°C(2373°F). ZIRCAR Refractory Sheet Type RS-MS Moldable Sleeving is odorless and contains no asbestos. Its high alumina content makes RS-MS highly resistant to many environments including molten aluminum as well as many types of fuel oils. When hardened with AL-Hard Refractory Sheet RS-MS become "rock hard" for greater strength. The many uses for Type RS-MS Sleeving include: cover for rings and saddles used in the annealing of hand blown glassware; asbestos sleeving replacement metal tube and pipe insulation; hose line and cable protection; and high temperature gaskets.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Thickness 1590 microns
62.5 mil
Thermal Properties Metric English Comments
Melting Point 1500 °C
2730 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Flammability Test 0.00
0.00
Nil
Component Elements Properties Metric English Comments
Al2O3 72 %
72 %
B2O3 3.0 %
3.0 %
CaO 6.0 %
6.0 %
Other <= 1.0 %
<= 1.0 %
SiO2 16 %
16 %
Processing Properties Metric English Comments
Moisture Content 40 %
40 %
Descriptive Properties Value Comments
Color White