LG Chemical LS170 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LS170 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Description: LS170, homopolymer made by suspension polymerization, is applied for value added products such as matted sheeting, super heat resistant wire ,high pressure hose, packing and gaskets for industrial supplies. It is used to enhance the mechanical property of the final good.Main Applications: Highly rigid heat-resistant power cable jacket, film, leather and sheet CAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D790
Bulk Density 0.460 - 0.540 g/cc
0.0166 - 0.0195 lb/in³
ASTM D1895
Volatiles <= 0.30 %

@Temperature 110 °C,
Time 3600 sec
<= 0.30 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 1600-1700
30°C, JIS K 6720-2
K-Value 76
DIN53726 / ISO1628-2