LG Chemical LS300 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LS300 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Description: LS300, a homopolymer made by suspension polymerization, is applied for value added special products such as matted sheeting ,super heat resistant wire, high pressure hose, packing and gasket for industrial supplies. It enhances the mechanical property of the final goods, and other high value added properties.Main Applications: Super heat-resistant power cable jacket and special gaskets of high elasticity and softness. CAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D790
Bulk Density 0.430 - 0.510 g/cc
0.0155 - 0.0184 lb/in³
ASTM D1895
Volatiles <= 0.30 %

@Temperature 110 °C,
Time 3600 sec
<= 0.30 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030
Particle Mesh Size 45 Mesh
45 Mesh
<0.2%; ASTM D1921
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 2500-2700
30°C, JIS K 6720-2
K-Value 84
DIN53726 / ISO1628-2