Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.430 g/cc | 0.0155 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons PUREX® HS 22 Carbon Black Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.430 - 0.510 g/cc | 0.0155 - 0.0184 lb/in³ | ASTM D1895 |
LG Chemical LS300 PVC General Description: LS300, a homopolymer made by suspension polymerization, is applied for value added special products such as matted sheeting ,super heat resistant wire, high pressure hose, packi.. |
|||
Bulk Density | 0.430 g/cc | 0.0155 lb/in³ | |
Solvay GEROPON® AF 71 Surfactant Description: "GEROPON AF 71 is powdered Foam Control Agent that has been developed for construction industry. GEROPON AF 71 depresses the formation of undesired air bubbles in building products, bas.. |
|||
Bulk Density | 0.430 g/cc | 0.0155 lb/in³ | |
Zircar Ceramics ECO-27A Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer.. |