Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LTL Color Compounds ColorFast® FRPC100 Polycarbonate, Flame-Retarded

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer LTL Color Compounds
Trade Name ColorFast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorFast® FRPC100 Polycarbonate, Flame-Retarded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
0.125; ASTM D955
Melt Flow 11 g/10 min

@Load 1.20 kg,
Temperature 300 °C
11 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Tensile Strength at Break 55.2 MPa
8000 psi
2.0 in/min; ASTM D638
Tensile Strength, Yield 62.1 MPa
9000 psi
2.0 in/min; ASTM D638
Elongation at Break 90 %
90 %
2.0 in/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2.0 in/min; ASTM D638
Flexural Strength 91.0 MPa
13200 psi
2.0 in/min; ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
2.0 in/min; ASTM D790
Izod Impact, Notched 6.41 J/cm

@Temperature 22.8 °C
12.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed (0.250"); ASTM D648
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Processing Properties Metric English Comments
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Nozzle Temperature 288 - 310 °C
550 - 590 °F
Melt Temperature 293 - 316 °C
560 - 600 °F
Mold Temperature 71.1 - 93.3 °C
160 - 200 °F
Drying Temperature 121 °C
250 °F
Dry Time 3 - 4 hour
3 - 4 hour
nominal; maximum drying time of 48 hours
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Shot Size 40 - 60 %
40 - 60 %
Vent Depth 0.00254 - 0.00762 cm
0.00100 - 0.00300 in
Screw Speed 40 - 70 rpm
40 - 70 rpm
Descriptive Properties Value Comments
UL File Number E178307
Users viewing this material also viewed the following: