Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Nylene® Naxel™ PC43 UV Resistant Polycarbonate Description: Naxel™ PC43 is a medium flow, UV resistant polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6 PA6 GR13 IM6 Glass Reinforced/Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | Tangent, Method B; ASTM D790 |
S&E Specialty Polymers GPP6100-116C PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 923 PC Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 923ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 678 ASA Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America F.. |
|||
Flexural Modulus | 2.24 - 2.55 GPa | 325 - 370 ksi | ASTM D790 |
Alcoa KAMA 4100 Prime APET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Ineos Nova FX550 (ASTM) Advanced Styrenic Polymer
(discontinued **) Extremely high glossHigh Izod impact strengthUL Classification 94 HBPractical toughnessHigh flow for injection moldingScuff resistanceApplications: Replacement resin for selected ABS applicationsRef.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 920ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML4539 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. Opaque colors. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | |
Kraton® G1652 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2mm/min; ASTM D790 |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Chase Plastics CP Pryme® N110GL (COND, 50% RH) Nylon 6, 10% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4001HH Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790A |
BP Amoco Accpro® 9934 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, Antistatic, High surface hardness, Stain resistanceComplies with FDA specification, Title 21, CFR 177.1520.Typica.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 940 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. |