Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSSâ„¢ A7 Mod. Wear-Resistant Tool Steel (ASTM A7 Mod.)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ A7 Mod. Wear-Resistant Tool Steel (ASTM A7 Mod.).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS A7 Mod. is a chromium-modified A7 type air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide particles in the steel. These carbides exhibit a hardness that is equivalent to approximately 80 to 85 Rockwell C. TLS A7 Mod. tool steel resists wear from sliding contact with other steels as well as from contact with dry and wet slurries of hard abrasive particles such as sand, shot blast media, and ceramics. Typical applications include brick mold liners, sand slinger liners, shot blasting equipment liners, extrusion tools for ceramics, powder compaction tooling, and machine tool ways.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 67
67
Air Cooled from 927°C, 30 minutes
68
68
Air Cooled from 982°C, 30 minutes
Machinability 20 - 25 %
20 - 25 %
1% Carbon Steel
Component Elements Properties Metric English Comments
Carbon, C 2.6 %
2.6 %
Chromium, Cr 8.25 %
8.25 %
Iron, Fe 82.545 %
82.545 %
Manganese, Mn 0.60 %
0.60 %
Molybdenum, Mo 1.2 %
1.2 %
Silicon, Si 0.30 %
0.30 %
Sulfur, S <= 0.0050 %
<= 0.0050 %
Vanadium, V 4.5 %
4.5 %