Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber/PTFE Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 180 MPa
26100 psi
Elongation at Yield 3.3 %
3.3 %
4.0 %
4.0 %
flexural
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 260 MPa
37700 psi
Flexural Modulus 8.50 GPa
1230 ksi
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
flatwise; ISO 179 1fU
4.50 J/cm²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.21
0.21
Coefficient of Friction, Static 0.17
0.17
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
DIN 53752
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 100 °C
212 °F
160 °C
320 °F
short term
Vicat Softening Point 245 °C
473 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color dark grey