Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1105-7096 PEEK, with carbon fiber, easy flowing

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-7096 PEEK, with carbon fiber, easy flowing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically conductive, suitable for continuous discharging of statically generated electricity.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm
0.00050 - 0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Stress 240 MPa
34800 psi
Elongation at Yield 1.5 %
1.5 %
2.0 %
2.0 %
flexural
Modulus of Elasticity 24.0 GPa
3480 ksi
Flexural Strength 350 MPa
50800 psi
Flexural Modulus 21.0 GPa
3050 ksi
Charpy Impact Unnotched 3.40 J/cm²
16.2 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Surface Resistance <= 1000 ohm
<= 1000 ohm
Insulation Resistance <= 1000 ohm
<= 1000 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black
Users viewing this material also viewed the following: