Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 350 MPa | 50800 psi | |
Pyrotek TS-180 Thermoset Electrical Insulation Product Glass reinforcement, Epoxy Resin, Straw Color. Excellent mechanical and electrical properties at elevated temperature.Information provided by Pyrotek. |
|||
Flexural Strength | 350 MPa | 50800 psi | ASTM D790 |
Gharda Chemicals GATONE™ 5630CF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Strength | 350 MPa | 50800 psi | |
Lehmann & Voss LUVOCOM® 20-0916 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Flexural Strength | 350 - 500 MPa | 50800 - 72500 psi | |
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Flexural Strength | 350 - 500 MPa | 50800 - 72500 psi | |
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
Flexural Strength | 350 - 500 MPa | 50800 - 72500 psi | |
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Flexural Strength | 350 - 500 MPa | 50800 - 72500 psi | |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Flexural Strength | 350 - 500 MPa | 50800 - 72500 psi | |
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi.. |
|||
Flexural Strength | 350 MPa | 50800 psi | |
Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 350 MPa | 50800 psi | 5 mm/min; ISO 178 |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |
|||
Flexural Strength | 350 MPa | 50800 psi | ASTM C1161 |
M Cubed Technologies ABC-501 Aluminum alloy-50% B4C Metal Matrix Composite Used for applications requiring neutron absorption. Unique process yields very high B4C content. Can be used to produce large, complex shapesInformation provided by M Cubed Technologies, Inc. |
|||
Flexural Strength | >= 350 MPa | >= 50800 psi | ASTM F417 |
CoorsTek AIN-170 Hot Pressed Aluminum Nitride Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors H.. |
|||
Flexural Strength | 350 MPa | 50800 psi | MOR; ASTM-F417 |
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia Oxygen ionic conductor for extreme-stress and extreme-thermal-shock environments |
|||
Flexural Strength | 350 MPa @Diameter >=100 mm |
50800 psi @Diameter >=3.94 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1 |
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications.. |
|||
Flexural Strength | 350 MPa @Diameter >=100 mm |
50800 psi @Diameter >=3.94 in |
24hr/23°C/50% RH, 230 Mpa measured at 150°C; ISO 178; IEC/EN 61212-2 5.1 |
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Flexural Strength | 350 MPa @Temperature 23.0 °C |
50800 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® 600 n Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Flexural Strength | 350 MPa | 50800 psi | ISO 178 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Strength | 350 MPa | 50800 psi | ASTM D790 |
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Flexural Strength | 350 MPa | 50800 psi | |
CeramTec Rubalit® A 1896 brown Alumina CeramTec AG's seal and regulator discs are made mainly of Rubalit® A 1896, a material developed especially for this application that is noted for the following special properties: outstanding hard.. |
|||
Flexural Strength | 350 MPa | 50800 psi | |
Lehmann & Voss LUVOCOM® 1105-7096 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |