Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resistance parts, hydrolysis resistance, non flammable.Antistatic.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Melt Flow <= 15.5 g/10 min

@Load 10.0 kg,
Temperature 380 °C
<= 15.5 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 180 MPa
26100 psi
Elongation at Yield 1.8 %
1.8 %
2.2 %
2.2 %
flexural
Modulus of Elasticity 17.0 GPa
2470 ksi
Flexural Strength 260 MPa
37700 psi
Flexural Modulus 15.0 GPa
2180 ksi
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
280 °C
536 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+8 - 1.00e+12 ohm
1.00e+8 - 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)