Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Stress 170 MPa
24700 psi
Elongation at Yield 1.5 %
1.5 %
1.7 %
1.7 %
flexural
Modulus of Elasticity 25.0 GPa
3630 ksi
Flexural Strength 230 MPa
33400 psi
Flexural Modulus 24.0 GPa
3480 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
edgewise; ISO 179 1eU
Coefficient of Friction, Dynamic 0.25
0.25
Coefficient of Friction, Static 0.20
0.20
Thermal Properties Metric English Comments
Thermal Conductivity 4.00 W/m-K
27.8 BTU-in/hr-ft²-°F
HOT-DISK || 60x60x3 mm
Maximum Service Temperature, Air 250 °C
482 °F
260 °C
500 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+7 ohm
>= 1.00e+7 ohm
Insulation Resistance >= 1.00e+7 ohm
>= 1.00e+7 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)