Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | 400 um thick sheet; ISO D-257 |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+17 ohm | 1.00e+7 - 1.00e+17 ohm | Average value: 2.12e+16 ohm Grade Count:26 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | ASTM D257 |
Kolon KOCETAL® CF702 Conductive Grade Acetal Resin Carbon fiber added, high stiffness and conductive grade. Applications: Conductive products. Information provided by API-Kolon. |
|||
Surface Resistance | 1.00e+7 - 1.00e+11 ohm | 1.00e+7 - 1.00e+11 ohm | IEC 60093 |
LG Chemical LUCON CP6080LP PC+CNT+GF Description: Injection Molding, PC+CNT+GF, Electrostatic Dissipation, Low Surface TribochargeApplication: ATM parts, HDD BracketCAS No. 103598-77-2, 65997-17-3 and 7782-42-5Information provided by L.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | |
Lord Adhesives Chemglaze® 9974 Roller Additive Chemglaze® thinners are formulated with urethane grade solvents and are used to reduce viscosity, aid bubble release, minimize orange peel, and make application easier.Chemglaze 9974 additive is .. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | ASTM D257 |
Techmer ES Electrablend® PC CF20 CR X 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Good Chemical Resistance and Semi ConductiveInformation provided by TP Compos.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant. |
|||
Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Surface Resistance | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
Techmer ES Statiblend® POM CO Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | 40% let-down in HDPE |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+11 ohm | 1.00e+7 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | 40% let-down in HDPE |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | 40% let-down in HDPE |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Surface Resistance | <= 1.00e+7 ohm @Temperature 23.0 °C |
<= 1.00e+7 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | IEC 60093 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | IEC 60093 |
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | DIN IEC 60093 |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | ASTM D257 |
Adamas Adalon® 305 PTFE, 15% Graphite Information provided by Adamas, HPM |