Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable for metall inserts.Improved friction and wear behaviour. Emergency running property.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
ISO 1183
Water Absorption <= 0.050 %
<= 0.050 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 130 MPa
18900 psi
Elongation at Yield 1.0 %
1.0 %
1.35 %
1.35 %
flexural
Modulus of Elasticity 17.0 GPa
2470 ksi
Flexural Strength 190 MPa
27600 psi
Flexural Modulus 14.0 GPa
2030 ksi
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
240 °C
464 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Electrical Properties Metric English Comments
Insulation Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Nozzle Temperature 320 - 340 °C
608 - 644 °F
Zone 1 300 - 320 °C
572 - 608 °F
Zone 2 310 - 330 °C
590 - 626 °F
Zone 3 320 - 340 °C
608 - 644 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color dark grey
Users viewing this material also viewed the following: