Less Common Metals Terbium Sublimed Rare Earth Metal

Category Metal , Nonferrous Metal , Pure Element
Manufacturer Less Common Metals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Less Common Metals Terbium Sublimed Rare Earth Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LCM manufactures a wide range of high purity rare earth metals plus yttrium and scandium. The metals are produced by reduction of suitable precursor materials followed by vacuum remelting and/or sublimination to give required purities.Form: Typically supplied in the form of irregular, broken or cropped ingot pieces.
Component Elements Properties Metric English Comments
Other <= 0.050 %
<= 0.050 %
Rare Earths <= 0.10 %
<= 0.10 %
Terbium, Tb >= 99.85 %
>= 99.85 %