Loctite® Varidot™ 3614 Stencil Print

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name Varidot™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Varidot™ 3614 Stencil Print.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application techniques including syringe dispense, stencil print and pin transfer.Loctite® syringe dispense products provide good performance for electronics assembly:High Speed DispenseLow Temperature CureProducts for difficult-to-bond substratesLoctite® 3614 Varidot™ Stencil PrintSpecifically formulated for Varidot™ and metal stencil print applications. Especially well suited for large components.Peaked dot profile. Process Method:Varidot Stencil Print (0.5-2"/sec.) Storage (Protect from heat): 40°F (+/-5°F) or 5°C (+/-3°C)
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 150 °C
0.0167 hour

@Temperature 302 °F
1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Shelf Life 9.00 Month
9.00 Month
From date of manufacture
Descriptive Properties Value Comments
Color Red