Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANLENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2.Applications: Coating for all substratesAdditives: BarefootAdvantages: Excellent drawdown Good heat seal ability and adhesion propertiesInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Water Vapor Transmission 18.5 g/m²/day
1.19 g/100 in²/day
90%RH, 37.8°C, 25µ; ASTM F372
Oxygen Transmission 230 cc-mm/m²-24hr-atm
584 cc-mil/100 in²-24hr-atm
ASTM D3985
Base Resin Melt Index 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Neck In 9.00 cm
3.54 in
Constant output 50m/min, 295°C; Internal Method
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
resin; ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 270 - 340 °C
518 - 644 °F